Обозначение | Заглавие на русском языке | Статус | Язык документа | Цена (с НДС 20%) в рублях |
|
Glass viscosity measurement—Rotational viscometer method
|
Published |
На языке оригинала
|
1310,00
|
|
|
Test method for melt viscosity of glass
|
Published |
На языке оригинала
|
1210,00
|
|
|
Test method for compression properties of continuous fiber reinforced ceramic matrix composites at high temperature
|
Published |
На языке оригинала
|
1814,00
|
|
|
Test method of temperature coefficient of infrared refractive index for infrared optical glass —Normal incidence method
|
Published |
На языке оригинала
|
1310,00
|
|
|
Test method for spherical indentation strength of porous ceramics
|
Published |
На языке оригинала
|
1210,00
|
|
|
Electronic dyed liquid crystal dimmable glass
|
Published |
На языке оригинала
|
2066,00
|
|
|
Test method for equibiaxial flexural strength of fine ceramics at room temperature—Ring-on-ring method
|
Published |
На языке оригинала
|
1310,00
|
|
|
Terms of smart glass
|
Published |
На языке оригинала
|
1562,00
|
|
|
High purity opaque quartz glass
|
Published |
На языке оригинала
|
1210,00
|
|
|
Self-cleaning coated glass for solar photovoltaic and solar-thermal generation
|
Published |
На языке оригинала
|
1562,00
|
|
|
Injection vials made of moulded glass
|
Published |
На языке оригинала
|
1411,00
|
|
|
Pharmaceutical glass tube
|
Published |
На языке оригинала
|
1210,00
|
|